FG2744 Superalloy Sintered Tube Filter

Catalog No. FG2744
Material Superalloy powder
Appearance Metallic tube
Working Temperature ≤900℃

Superalloy Sintered Tube Filter has a great heat resistance and can easily work under a temperature of 900 ℃. Stanford Advanced Materials is a global manufacturer of high-quality sintered metal products like Superalloy Sintered Tube Filters.

Related Products:IF1797 Gas Pressure Sintering FurnaceMF2361 Stainless Steel Fiber Sintered FeltMF1448 Sintered LaminatesMF2362 Hastelloy Fiber Media

Superalloy Sintered Tube Filter Description

Made through CIP and sintering process, the Sintered Tube Filter demonstrates high tensile strength, high compressive strength, great heat and corrosion resistance, low initial pressure differential, and great permeability. Based on the filter media, suitable material shall be used to produce Sintered Tube Filters.

Superalloy Sintered Tube Filter Specification

Product Name

Sintered Tube Filter

Size of seamless tube (Outer Diameter Wall ThicknessLength)

20×2×(30-300),

30×2×(50-500),

35×2×(50-1000),

40×2×(50-1000),

50×2.5×(50-1500),

60×2.5×(100-2000),

65×2.5×(100-2000),

75×3×(100-1800),

80×3×Length(customizable),

90×3.5×Length(customizable), etc

Type of interface

Threaded interface:

G1/2、G3/4、M20、M30、M36、M42, etc

Filter element interface:

215, 220, 222, 226, Pressure Filter, etc

Flange interface

Different types of interface can be customized under agreement.

Superalloy Sintered Tube Filter Applications:

 

Example

Filter made of stainless steel

Mode

Size of blocked particle under 98% filtration efficiency

(μm)

Size of blocked particle under 99.9% filtration efficiency

(μm)

 

Permeability 

(10-12m^2)

Relative gas permeability 

[m^3/(h·kPa·m^2)]

Mpa

ADSG-3

3

5

0.18

≥18

3

ADSG-10

10

15

0.9

≥90

3

ADSG-20

25

35

4

≥400

3

ADSG-60

50

80

7.5

≥750

2.5

Note: The permeability in the above examples corresponds to filters with wall thickness of 2mm.

LATEST RECOMMENDED

TF2192 PTFE Filter Bag

TF2192 PTFE Filter Bag

FG2738 316L Sintered Tube Filter

FG2738 316L Sintered Tube Filter

FG2739 430 Sintered Tube Filter

FG2739 430 Sintered Tube Filter

FG2740 904L Sintered Tube Filter

FG2740 904L Sintered Tube Filter

FG2741 C-276 Sintered Tube Filter

FG2741 C-276 Sintered Tube Filter

FG2742 Duplex Stainless Steel Sintered Tube Filter

FG2742 Duplex Stainless Steel Sintered Tube Filter

FG2743 MONEL Sintered Tube Filter

FG2743 MONEL Sintered Tube Filter

FG2745 Titanium Sponge Powder Sintered Tube Filter

FG2745 Titanium Sponge Powder Sintered Tube Filter

GET A QUOTE

Please fill in your details and one of our material experts will get back to you within 24 hours. For more information, contact us via E-mail at sales@samaterials.com.

** Email address with your company's domain name is preferred. Otherwise, we may not be able to process your inquiry.