Composite Ion Exchange Membrane Description
Composite Ion Exchange Membrane (electrolysis and electroplating) uses high-strength polytetrafluoroethylene mesh as the support layer, and is matched with perfluorosulfonic acid resin with appropriate molecular weight and ion exchange capacity to form a composite membrane with uniform thickness.
Composite Ion Exchange Membranes (CIEMs) offer significant advantages over traditional membranes by combining the best properties of multiple materials. They play a crucial role in energy storage (flow batteries), power generation (fuel cells), and water purification. Their ability to improve selectivity, conductivity, and durability makes them essential for sustainable technologies, particularly in renewable energy systems and industrial water treatment.
Composite Ion Exchange Membrane Specification
Thickness & Gram Weight
Model
|
Thickness (μm)
|
Gram Weight (g/m²)
|
N-417
|
260
|
340
|
N-4110
|
360
|
470
|
Physical and Other Properties
Physical Properties
Tensile Test (23°C, 50% RH)
|
Technical Indicators
|
Tensile Strength (MPa)
|
≥40
|
Elongation at break (%)
|
≥3100
|
Specific Gravity
|
1.35
|
Conductivity (S/cm)
|
>0.100
|
Acid capacity (meq/g)
|
1.00±0.05
|
Swelling Performance
Swelling Performance
|
Technical Indicators
|
Water content (%)
|
5.0±3.0
|
Water absorption rate (%)
|
50.0±5.0
|
(23℃,50% RH) Thickness Swelling Rate
|
water soaked at 23℃ 50% RH
|
≤5
|
water soaked at 100℃ 50% RH
|
≤10
|
Linear expansion,% increase (23℃,50% RH)
|
Soaked at 23℃, 50% RH
|
≤2
|
Soaked at 100℃, 50% RH
|
≤5
|
Composite Ion Exchange Membrane Application
Composite Ion Exchange Membrane is widely used in electrolytic chlorine dioxide generators, copper recovery in etching solution, preparation of gold salts, amino acid refining, caustic soda preparation, electrodialysis, and other electrolytic and electroplating industries.
Composite Ion Exchange Membrane Packing
Our Composite Ion Exchange Membrane (electrolysis and electroplating) is carefully handled during storage and transportation to preserve the quality of our product in its original condition.
Specification
Thickness & Gram Weight
Model
|
Thickness (μm)
|
Gram Weight (g/m²)
|
N-417
|
260
|
340
|
N-4110
|
360
|
470
|
Physical and Other Properties
Physical Properties
Tensile Test (23°C, 50% RH)
|
Technical Indicators
|
Tensile Strength (MPa)
|
≥40
|
Elongation at break (%)
|
≥3100
|
Specific Gravity
|
1.35
|
Conductivity (S/cm)
|
>0.100
|
Acid capacity (meq/g)
|
1.00±0.05
|
Swelling Performance
Swelling Performance
|
Technical Indicators
|
Water content (%)
|
5.0±3.0
|
Water absorption rate (%)
|
50.0±5.0
|
(23℃,50% RH) Thickness Swelling Rate
|
water soaked at 23℃ 50% RH
|
≤5
|
water soaked at 100℃ 50% RH
|
≤10
|
Linear expansion,% increase (23℃,50% RH)
|
Soaked at 23℃, 50% RH
|
≤2
|
Soaked at 100℃, 50% RH
|
≤5
|