250mL Yttria Stabilized Zirconia Jar with Lid Description:
Zirconia ceramics performance:
Density: 6.05 g/cm3
Water absorption: <0.05%
Firing temperature: 1550 °C
Hardness: 1350 HV
Bending strength: 950 MPa
Compression strength: 25000 MPa
Breaking tenacity: 6-8 Mpa•m1/2
Hot expansion coefficient: 9.5x10-6 /°C
Other names for Yttria Stabilized Zirconia Jar: Yttria Stabilized Zirconia Grinding Jar (YSZ Grinding Jar), Zirconia Jar and Zirconium Oxide Jar.
Advantages of Yttria Stabilized Zirconia Grinding Jar and Grinding Media Include:
- High density
- High hardness and toughness, 60 times the hardness of regular steel
- High thermal expansion
- Low thermal conductivity
- Impact resistance
- High corrosion and wear resistance

250mL Yttria Stabilized Zirconia Jar with Lid Specifications:
|
TYPE-MQ
|
TYPE-GT
|
Capacity
|
250ml
|
250ml
|
Outer Diameter
|
94mm
|
91mm
|
Height
|
82mm
|
78mm
|
Wall Thickness
|
8mm
|
8mm
|
Lid Thickness
|
7mm
|
7mm
|
The above dimensions are for your reference. Contact us for precise specifications or tailor-made requests.
*Grinding Ball Recommendation: When you use 250mL YSZ jar, 280pcs of Dia. 5mm balls or 40pcs of Dia. 10mm balls are recommended.
250mL Yttria Stabilized Zirconia Jar with Lid Applications:
- Yttria Stabilized Zirconia / YSZ grinding jars are used to grind materials into extremely fine powder for use in mineral dressing processes, paints, pyrotechnics, ceramics and selective laser sintering.
- Zirconia jars and Zirconia balls are strong and have good abrasion resistance, which prevents mixing with other impurities while ball mill grinding.
250mL Yttria Stabilized Zirconia Jar with Lid Packaging:
SAM’s Zirconia grinding jars and YSZ grinding jars are carefully handled to minimize damage during storage and transportation and to preserve the quality of our products in their original condition.
Material Safety Data Sheet (MSDS) for your reference!