LM4521 NCM811 Cathode Precursor (Nickel-Cobalt-Manganese)

Catalog No. LM4521
BET 16±3.0 m2/g
Tap Density 1.65±0.15 g/cm3
Bulk Density 1.10±0.2 g/cm3

NCM811 Cathode Precursor (Nickel-Cobalt-Manganese) is prepared by the co-precipitation method after adjusting the molar ratio of transition metal ions. Stanford Advanced Materials (SAM) has rich experience in manufacturing and supplying high-quality NCM811 Cathode Precursor (Nickel-Cobalt-Manganese).

Related products: Lithium Iron Phosphate Powder LiFePO4, LFP, Lithium Cobalt (III) Oxide Powder (LCO Powder), Lithium Manganese Oxide Powder (LMO Powder), NCM523 Cathode Precursor, NCM622 Cathode Precursor

NCM811 Cathode Precursor (Nickel-Cobalt-Manganese) Description

NCM811 Cathode Precursor (Nickel-Cobalt-Manganese) is prepared by the co-precipitation method after adjusting the molar ratio of transition metal ions. They are used to synthesize NCM Lithium Nickel Cobalt Aluminum Oxide Cathode. Most of the precursors have sphere morphology.

NCM811 Cathode Precursor (Nickel-Cobalt-Manganese) Specifications

Item

Unit

Value

D10

um

>2.2

D50

um

3.9±0.2

D90

um

<6.4

BET

m2/g

16±3.0

Tap Density

g/cm3

1.65±0.15

Bulk Density

g/cm3

1.10±0.2

Ni

wt%

51.44±1.0

Co

wt%

7.00±0.3

Mn

wt%

3.56±0.3

NCM811 Cathode Precursor (Nickel-Cobalt-Manganese) Applications

NCM811 Cathode Precursor (Nickel-Cobalt-Manganese) is applied in the lithium-ion battery for the electric vehicle, electric tool, and 3C device.

NCM811 Cathode Precursor (Nickel-Cobalt-Manganese) Packaging

Our NCM811 Cathode Precursor (Nickel-Cobalt-Manganese) is carefully handled during storage and transportation to preserve the quality of our product in its original condition.

LATEST RECOMMENDED

sc/1656484196-normal-Lithium Dichromate Hydrate.jpg

LM4242 Lithium Dichromate Hydrate Powder (CAS No. 52478-50-9)

sc/1669860080-normal-high-magnification-nmc-ternary-cathode-material.jpg

LM4513 High-magnification NMC Ternary Cathode Material (NCM523)

sc/1669860858-normal-monocrystalline-nmc-ternary-cathode-material-high-power-ncm523.jpg

LM4514 Monocrystalline NMC Ternary Cathode Material (High-power NCM523)

sc/1669861297-normal-monocrystalline-nmc-ternary-cathode-material-high-power-ncm622.jpg

LM4515 Monocrystalline NMC Ternary Cathode Material (High-power NCM622)

sc/1669861579-normal-lithium-cobalt-oxide-cathode-material-lco-powder.jpg

LM4516 Lithium Cobalt Oxide Cathode Material (LCO Powder)

sc/1669861857-normal-lnmo-cathode-powder.jpg

LM4517 LNMO Cathode Powder

sc/1669864307-normal-NCM523 Cathode Precursor (Nickel-Cobalt-Manganese).jpg

LM4519 NCM523 Cathode Precursor (Nickel-Cobalt-Manganese)

sc/1669865275-normal-NCM622 Cathode Precursor (Nickel-Cobalt-Manganese).jpg

LM4520 NCM622 Cathode Precursor (Nickel-Cobalt-Manganese)

sc/1669866312-normal-Lithium Aluminum Titanium Phosphate Electrolyte sheet.jpg

LM4522 Lithium Aluminum Titanium Phosphate Electrolyte sheet (LATP)

GET A QUOTE

Please fill in your details and one of our material experts will get back to you within 24 hours. For more information, contact us via E-mail at sales@samaterials.com.

** Email address with your company's domain name is preferred. Otherwise, we may not be able to process your inquiry.

 Inquiry List
1